Articles
DOI DOI: 10.62441/actainnovations.vi.3052

EFFECT OF CEO2 AND LA2O3 REINFORCEMENTS ON MECHANICAL, TRIBOLOGICAL AND MICROSTRUCTURAL PROPERTIES OF WC–12CO COATING BY HIGH-VELOCITY OXYGEN FUEL DEPOSITION TECHNIQUE

Abstract

Decarburization during HVOF deposition reduces the workability of Tungsten Carbide-12% Cobalt (WC-12Co) coatings. This work examines how CeO2 and La2O3 reinforcements affect HVOF-sprayed WC-12Co coatings' mechanical, tribological, and microstructural characteristics. Compared to the unreinforced coating, microstructure, phase composition, bond strength, abrasive wear, coefficient of friction, and microhardness were assessed. CeO2 or La2O3 decreased porosity and finer grain structure without affecting bond strength. Coatings with 1 wt.% CeO2 and La2O3 increased microhardness by 6% and 4%, respectively, compared to the unreinforced WC-12Co coating, which had an adhesive bond strength of 73.60 ± 5 MPa. Both changed coatings improved structural stability, grain refinement, and densification. Minimum wear rate of 3.5 × 10⁻⁵ mm³/N·m was found in WC-12Co-1La2O3, whereas the lowest coefficient of friction was 0.4 in WC-12Co-1CeO2. An oxide layer from reinforcements enhanced wear resistance. SEM investigation of worn surfaces showed debris, dislodged carbide particles, SiC grains, microcracks, and grooves as the predominant wear processes.

How to Cite

Dubey , S., Birla , S., & Mishra , T. K. (2026). EFFECT OF CEO2 AND LA2O3 REINFORCEMENTS ON MECHANICAL, TRIBOLOGICAL AND MICROSTRUCTURAL PROPERTIES OF WC–12CO COATING BY HIGH-VELOCITY OXYGEN FUEL DEPOSITION TECHNIQUE. ACTA INNOVATIONS, 450–464. https://doi.org/10.62441/actainnovations.vi.3052

References

  1. 1. Babu, P.S., et al., Coatability and performance evaluation of TiN-Ni composite coatings by detonation spray technique. Ceramics International, 2026.
  2. 2. Yang, C.-g., et al., A novel plasma-enhanced high-velocity arc spraying technique for the efficient and high-quality deposition of Ni-based coatings. Journal of Alloys and Compounds, 2026: p. 187449.
  3. 3. Kumar, K., S. Kumar, and H.S. Gill, Role of carbide-based thermal-sprayed coatings to prevent failure for boiler steels: a review. Journal of Failure Analysis and Prevention, 2024. 24(4): p. 1628–1663.
  4. 4. Torkashvand, K., S. Joshi, and M. Gupta, Advances in thermally sprayed WC-based wear-resistant coatings: co-free binders, processing routes and tribological behavior. Journal of Thermal Spray Technology, 2022. 31(3): p. 342–377.
  5. 5. Vashishtha, N., R. Khatirkar, and S. Sapate, Tribological behaviour of HVOF sprayed WC-12Co, WC-10Co-4Cr and Cr3C2− 25NiCr coatings. Tribology international, 2017. 105:
  6. p. 55–68.
  7. 6. Mishra, T.K., A. Kumar, and S. Sinha, Experimental investigation and study of HVOF sprayed WC-12Co, WC-10Co-4Cr and Cr3C2-25NiCr coating on its sliding wear behaviour. International Journal of Refractory Metals and Hard Materials, 2021. 94: p. 105404.
  8. 7. Mi, P. and F. Ye, Structure and wear performance of the atmospheric heat-treated HVOF sprayed bimodal WC-co coating. International Journal of Refractory Metals and Hard Materials, 2018. 76: p. 185–191.
  9. 8. Asgari, H., G. Saha, and M. Mohammadi, Tribological behavior of nanostructured high velocity oxy-fuel (HVOF) thermal sprayed WC-17NiCr coatings. Ceramics International, 2017. 43(2): p. 2123–2135.
  10. 9. Fu, W., et al., Microstructure and properties of high velocity oxygen fuel sprayed (WC-Co)-Ni coatings. Ceramics International, 2020. 46(10): p. 14940–14948.
  11. 10. Jadidi, M., S. Moghtadernejad, and A. Dolatabadi, A comprehensive review on fluid dynamics and transport of suspension/liquid droplets and particles in high-velocity oxygen-fuel (HVOF) thermal spray. Coatings, 2015. 5(4): p. 576–645.
  12. 11. Wang, T. and F. Ye, The elevated-temperature wear behavior evolution of HVOF sprayed tungsten carbide coatings: Respond to heat treatment. International Journal of Refractory Metals and Hard Materials, 2018. 71: p. 92–100.
  13. 12. Pan, S., et al., Metal matrix nanocomposites in tribology: Manufacturing, performance, and mechanisms. Friction, 2022. 10(10): p. 1596–1634.
  14. 13. Ji, D.-H., et al., Effect of abrasive particle size on the tribological behavior of thermal sprayed WC-Cr3C2-Ni coatings. Journal of Alloys and Compounds, 2022. 924: p. 166536.
  15. 14. Rajinikanth, V. and K. Venkateswarlu, An investigation of sliding wear behaviour of WC–Co coating. Tribology International, 2011. 44(12): p. 1711–1719.
  16. 15. Wang, H., et al., Sliding wear resistance enhancement by controlling W2C precipitation in HVOF sprayed WC-based cermet coating. Surface and Coatings Technology, 2020. 387:
  17. p. 125533.
  18. 16. Sarkar, S. and P.P. Bandyopadhyay, Effect of in-flight particle parameters on friction and wear characteristics of HVOF-sprayed WC-12Co coatings fabricated from conventional and submicron-sized carbide grits. Wear, 2026: p. 206624.
  19. 17. Lim, N., et al., Fabrication and microstructural characterization of nano-structured WC/Co coatings. Surface and Coatings Technology, 2010. 205(2): p. 430–435.
  20. 18. Song, B., et al., Dry sliding wear behaviour of HVOF thermal sprayed WC-Co-Cr and WC-CrxCy-Ni coatings. Wear, 2020. 442: p. 203114.
  21. 19. Badiee, F., et al., Wear behaviour assessment of sol-enhanced Ni–P/Ni–B–CeO2 nanocomposite coatings. Results in Surfaces and Interfaces, 2026: p. 100894.
  22. 20. Wang, K., et al., Rare earth elements modification of laser-clad nickel-based alloy coatings. Applied surface science, 2001. 174(3-4): p. 191–200.
  23. 21. Guo, Z., et al., Research status of ceramic coatings prepared by laser cladding. The International Journal of Advanced Manufacturing Technology, 2025. 141(9): p. 4671–4699.
  24. 22. Liu, Y., et al., Effects of rare earth elements on the microstructure and mechanical properties of HVOF-sprayed WC-Co coatings. Journal of thermal spray technology, 2014. 23(7): p. 1225–1231.
  25. 23. Zhang, Z., et al., Effect of CeO2 on the microstructure and wear behavior of thermal spray welded NiCrWRE coatings. Wear, 2007. 262(5-6): p. 562–567.
  26. 24. Liu, Y., et al., Influence of rare earth on the high-temperature sliding wear behavior of WC-12Co coating prepared by HVOF spraying. Journal of Thermal Spray Technology, 2018. 27(7): p. 1143–1152.
  27. 25. Ding, X., et al., Microstructure and wear performance of CeO2-modified micro-nano structured WC-CoCr coatings sprayed with HVOF. Lubricants, 2023. 11(5): p. 188.
  28. 26. Zhang, F., et al., Microstructure, mechanical properties and wear resistance of rare earth doped WC/steel matrix composites: Experimental and calculations. Ceramics International, 2023. 49(2): p. 2638–2647.
  29. 27. Kishore, M.T., K. Arbind, and S.S. Kumar, Sliding wear behaviour of thermally sprayed WC–20Cr3C2–7Ni and La2O3 composite coatings. Emerging Materials Research, 2021. 10(4): p. 348–356.
  30. 28. Du, J., et al., The influence of nano-CeO2 on tribological properties and microstructure evolution of Cr3C2-NiCrCoMo composite coatings at high temperature. Surface and Coatings Technology, 2021. 428: p. 127913.
  31. 29. Fu, D., H. Xiong, and Q. Wang, Microstructure evolution and its effect on the wear performance of HVOF-sprayed conventional WC-Co coating. Journal of Materials Engineering and Performance, 2016. 25(10): p. 4352–4358.
  32. 30. Miao, L., et al., Effect of CeO2 Addition on the Microstructure and Properties of Induction Heating Ni-WC-CeO2 Composite Coatings. Materials, 2025. 18(10): p. 2175.
  33. 31. Ding, L. and S. Hu, Effect of nano-CeO2 on microstructure and wear resistance of Co-based coatings. Surface and Coatings Technology, 2015. 276: p. 565–572.
  34. 32. Chauhan, H.R., et al., Role of micro-and nano-CeO2 reinforcements on characteristics and tribological performance of HVOF sprayed Cr3C2-NiCr coatings. Surface and Coatings Technology, 2023. 467: p. 129684.
  35. 33. Zhang, W., et al., Preparation and investigation of Ni-W/CeO2 composite coating and its structure and anti-corrosion properties with different ceria content and deposition time. Ceramics International, 2024. 50(21): p. 44560–44571.
  36. 34. Tillmann, W., et al., Sliding and rolling wear behavior of HVOF-sprayed coatings derived from conventional, fine and nanostructured WC-12Co powders. Journal of thermal spray technology, 2014. 23(1): p. 262–280.
  37. 35. Xie, M., S. Zhang, and M. Li, Comparative investigation on HVOF sprayed carbide-based coatings. Applied Surface Science, 2013. 273: p. 799–805.
  38. 36. Singh, V., et al., Development and performance evaluation of La2O3 doped WC-10Co-4Cr coatings for enhanced biofouling and slurry abrasion resistance. Journal of Materials Research and Technology, 2025.
  39. 37. Yang, F., et al., Reducing sintering cracks in oxide/oxide ceramic matrix composites via oxidation-induced expansion of zirconium carbide. Ceramics International, 2025. 51(25):
  40. p. 43737–43748.Li, W., et al., Mechanistic insights into CeO₂-induced microstructure refinement and oxidative wear regulation in laser-deposited WC-12Co composite coatings. Materials Characterization, 2026: p. 116604.
  41. 38. Shu, D., et al., Influence of CeO2 content on WC morphology and mechanical properties of WC/Ni matrix composites coating prepared by laser in-situ synthesis method. Journal of Materials Research and Technology, 2020. 9(5): p. 11111–11120.
  42. 39. Lakkannavar, V., et al., Thermal spray coatings on high-temperature oxidation and corrosion applications–a comprehensive review. Results in Surfaces and Interfaces, 2024. 16: p. 100250.
  43. 40. Wang, H., et al., Wear resistance enhancement of HVOF-sprayed WC-Co coating by complete densification of starting powder. Materials & Design, 2020. 191: p. 108586.
  44. 41. Wei, Z.-Y., et al., Progress in ceramic materials and structure design toward advanced thermal barrier coatings. Journal of Advanced Ceramics, 2022. 11(7): p. 985–1068.
  45. 42. Farahmand, P., et al., Laser cladding assisted by induction heating of Ni–WC composite enhanced by nano-WC and La2O3. Ceramics International, 2014. 40(10): p. 15421–15438.
  46. 43. Farokhzadeh, K., R. Fillion, and A. Edrisy, The effect of deposition rate on microstructural evolution in WC-Co-Cr coatings deposited by high-velocity oxy-fuel thermal spray process. Journal of Materials Engineering and Performance, 2019. 28(12): p. 7419–7430.
  47. 44. Liu, Y., et al., Effect of carbon content on microstructures, mechanical and tribological properties and thermal stability in WBC films. Surface and Coatings Technology, 2016. 291: p. 276–285.
  48. 45. Wahab, M., Importance of d-Spacing in Diffraction of Crystals, in Mirror Symmetry: The Mother of all Crystal Symmetries. 2024, Springer. p. 105–142.
  49. 46. Solodkyi, I., et al., Hardmetals prepared from WC-W2C eutectic particles and AlCrFeCoNiV high entropy alloy as a binder. Vacuum, 2022. 195: p. 110630.
  50. 47. Kaschel, F., et al., Mechanism of stress relaxation and phase transformation in additively manufactured Ti-6Al-4V via in situ high temperature XRD and TEM analyses. Acta Materialia, 2020. 188: p. 720–732.
  51. 48. Zhu, Y., et al., Effect of nanoscale CeO2 powder on wear and corrosion resistance of Ni60A-WC coatings. Ceramics International, 2025. 51(8): p. 10913–10932.
  52. 49. Wu, B., et al., Rare earth elements in cast aluminum alloys: Microstructural control and performance enhancement. Journal of Rare Earths, 2025.
  53. 50. Van Steenkiste, T., J. Smith, and R. Teets, Aluminum coatings via kinetic spray with relatively large powder particles. Surface and Coatings Technology, 2002. 154(2-3): p. 237–252.
  54. 51. Jiang, H., et al., Coprecipitation of Co and La2O3 coprecipitation on WC for tailoring the grain distribution and boundary of high-performance coarse-grained WC-10Co cemented carbide. International Journal of Refractory Metals and Hard Materials, 2023. 115: p. 106303.
  55. 52. Alidokht, S.A. and R.R. Chromik, Sliding wear behavior of cold-sprayed Ni-WC composite coatings: Influence OF WC content. Wear, 2021. 477: p. 203792.
  56. 53. Padilla II, H.A., et al., Frictional performance and near-surface evolution of nanocrystalline Ni–Fe as governed by contact stress and sliding velocity. Wear, 2013. 297(1-2): p. 860–871.
  57. 54. John, M. and P.L. Menezes, Self-lubricating materials for extreme condition applications.
  58. Materials, 2021. 14(19): p. 5588.Haque, T., et al., The role of abrasive particle size on the wear of diamond-like carbon coatings. Wear, 2013. 302(1-2): p. 882–889.
  59. 55. Shi, C., et al., High-Temperature Tribological Performance of Nano-Modified Multimodal Cr3C2-NiCr Coatings. Journal of Thermal Spray Technology, 2025. 34(8): p. 3322–3341.
  60. 56. Liu, Y., et al., The effect of temperature rise on the wear mechanisms of 3D-printed TC4 alloy under different loads and ambient temperatures. Materials Characterization, 2025: p. 115885.
  61. 57. Sharma, P., S.K. Mishra, and J. Ramkumar, Coupled Wear Mechanisms and Subsurface Deformation Evolution of Ti6Al4V in Contact with Novel Quaternary Nitride-Coated Cemented Carbide Tools. Ceramics International, 2026.